J C Lashley1, A C Lawson, J C Cooley, B Mihaila, C P Opeil, L Pham, W L Hults, J L Smith, G M Schmiedeshoff, F R Drymiotis, G Chapline, S Basu, P S Riseborough.
Abstract
The gamma-->alpha isostructural transition in the Ce0.9-xLaxTh0.1 system is measured as a function of La alloying using specific heat, magnetic susceptibility, resistivity, thermal expansivity or striction measurements. A line of discontinuous transitions, as indicated by the change in volume, decreases exponentially from 118 K to close to 0 K with increasing La doping, and the transition changes from being first-order to continuous at a critical concentration, x(c) approximately 0.14. At the tricritical point, the coefficient of the linear T term in the specific heat gamma and the magnetic susceptibility increase rapidly near x(c) and approach large values at x=0.35 signifying that a heavy Fermi-liquid state evolves at large doping. The Wilson ratio reaches a value above 2 for a narrow range of concentrations near x(c), where the specific heat and susceptibility vary most rapidly with the doping concentration.Year: 2006 PMID: 17280213 DOI: 10.1103/PhysRevLett.97.235701
Source DB: PubMed Journal: Phys Rev Lett ISSN: 0031-9007 Impact factor: 9.161