Bacterial degradation of poly(trans-1,4-isoprene) (gutta percha).

Sören Warneke1, Matthias Arenskötter, Klaus B Tenberge, Alexander Steinbüchel.   

Abstract

Gutta percha, the trans-isomer of polyisoprene, is being used for several technical applications due to its resistance to biological degradation. In the past, several attempts to isolate micro-organisms capable of degrading chemically pure poly(trans-1,4-isoprene) have failed. This is the first report on axenic cultures of bacteria capable of degrading gutta percha. From about 100 different habitats and enrichment cultures, six bacterial strains were isolated which utilize synthetic poly(trans-1,4-isoprene) as sole carbon and energy source for growth. All isolates were assigned to the genus Nocardia based on 16S rRNA gene sequences. Four isolates were identified as strains of Nocardia nova (L1b, SH22a, SEI2b and SEII5a), one isolate was identified as a strain of Nocardia jiangxiensis (SM1) and the other as a strain of Nocardia takedensis (WE30). In addition, the type strain of N. takedensis obtained from a culture collection (DSM 44801(T)) was shown to degrade poly(trans-1,4-isoprene). Degradation of poly(trans-1,4-isoprene) by these seven strains was verified in mineralization experiments by determining the release of CO(2). All seven strains were also capable of mineralizing poly(cis-1,4-isoprene) and to use this polyisoprenoid as a carbon and energy source for growth. Mineralization of poly(trans-1,4-isoprene) after 80 days varied from 3 % (strain SM1) to 54 % (strain SEI2b) and from 34 % (strain L1b) to 43 % (strain SH22a) for the cis-isomer after 78 days. In contrast, Gordonia polyisoprenivorans strain VH2, which was previously isolated as a potent poly(cis-1,4-isoprene)-degrading bacterium, was unable to degrade poly(trans-1,4-isoprene). Scanning electron microscopy revealed cavities in solid materials prepared from poly(trans-1,4-isoprene) and also from poly(cis-1,4-isoprene) after incubation with N. takedensis strain WE30 or with N. nova strain L1b, whereas solid poly(trans-1,4-isoprene) material remained unaffected if incubated with G. polyisoprenivorans strain VH2 or under sterile conditions.

Entities:  

Mesh:

Substances:

Year:  2007        PMID: 17259606     DOI: 10.1099/mic.0.2006/000109-0

Source DB:  PubMed          Journal:  Microbiology        ISSN: 1350-0872            Impact factor:   2.777


  9 in total

1.  Insights into the microbial degradation of rubber and gutta-percha by analysis of the complete genome of Nocardia nova SH22a.

Authors:  Quan Luo; Sebastian Hiessl; Anja Poehlein; Rolf Daniel; Alexander Steinbüchel
Journal:  Appl Environ Microbiol       Date:  2014-04-18       Impact factor: 4.792

2.  First report of cis-1,4-polyisoprene degradation by Gordonia paraffinivorans.

Authors:  Stefania Pegorin Braga; Alexandre Paes Dos Santos; Thais Paganini; Deibs Barbosa; George Willian Condomitti Epamino; Carlos Morais; Layla Farage Martins; Aline Maria Silva; João Carlos Setubal; Marcelo Afonso Vallim; Renata Castiglioni Pascon
Journal:  Braz J Microbiol       Date:  2019-08-22       Impact factor: 2.476

Review 3.  Historical and recent achievements in the field of microbial degradation of natural and synthetic rubber.

Authors:  Meral Yikmis; Alexander Steinbüchel
Journal:  Appl Environ Microbiol       Date:  2012-04-13       Impact factor: 4.792

4.  Involvement of two latex-clearing proteins during rubber degradation and insights into the subsequent degradation pathway revealed by the genome sequence of Gordonia polyisoprenivorans strain VH2.

Authors:  Sebastian Hiessl; Jörg Schuldes; Andrea Thürmer; Tobias Halbsguth; Daniel Bröker; Angel Angelov; Wolfgang Liebl; Rolf Daniel; Alexander Steinbüchel
Journal:  Appl Environ Microbiol       Date:  2012-02-10       Impact factor: 4.792

Review 5.  Ability of new obturation materials to improve the seal of the root canal system: a review.

Authors:  Guo-Hua Li; Li-Na Niu; Wei Zhang; Mark Olsen; Gustavo De-Deus; Ashraf A Eid; Ji-Hua Chen; David H Pashley; Franklin R Tay
Journal:  Acta Biomater       Date:  2013-12-07       Impact factor: 8.947

6.  Possible involvement of an extracellular superoxide dismutase (SodA) as a radical scavenger in poly(cis-1,4-isoprene) degradation.

Authors:  Carina Schulte; Matthias Arenskötter; Mahmoud M Berekaa; Quyen Arenskötter; Horst Priefert; Alexander Steinbüchel
Journal:  Appl Environ Microbiol       Date:  2008-10-24       Impact factor: 4.792

7.  Microbial gutta-percha degradation shares common steps with rubber degradation by Nocardia nova SH22a.

Authors:  Quan Luo; Sebastian Hiessl; Anja Poehlein; Alexander Steinbüchel
Journal:  Appl Environ Microbiol       Date:  2012-12-07       Impact factor: 4.792

8.  Functional identification of rubber oxygenase (RoxA) in soil and marine myxobacteria.

Authors:  Jakob Birke; Wolf Röther; Georg Schmitt; Dieter Jendrossek
Journal:  Appl Environ Microbiol       Date:  2013-08-09       Impact factor: 4.792

9.  Stability of Doxycycline Absorbed on Root Canal Dentin After Obturation with Gutta-Percha/AH26 and Resilon/RealSeal at Different Time Intervals.

Authors:  Behnam Bolhari; Naghmeh Meraji; Ali Nosrat; Shokoufeh Hassani
Journal:  J Dent (Tehran)       Date:  2013-05-31
  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.