| Literature DB >> 16853387 |
C-W Yi1, K Luo, T Wei, D W Goodman.
Abstract
Pd, Au, and Pd-Au mixtures were deposited via physical vapor deposition onto a Mo(110) substrate, and the surface concentration and morphology of the Pd-Au mixtures were determined by low-energy ion scattering spectroscopy (LEISS), infrared absorption spectroscopy (IRAS), temperature-programmed desorption (TPD), and X-ray photoelectron spectroscopy (XPS). Pd-Au mixtures form a stable alloy between 700 and 1000 K with substantial enrichment in Au compared to the bulk composition. Annealing a 1:1 Pd-Au mixture at 800 K leads to the formation of a surface alloy with a composition Au(0.8)Pd(0.2) where Pd is predominantly surrounded by Au. The surface concentration of this isolated Pd site can be systematically controlled by altering the bulk Pd-Au alloy concentration.Entities:
Year: 2005 PMID: 16853387 DOI: 10.1021/jp053515r
Source DB: PubMed Journal: J Phys Chem B ISSN: 1520-5207 Impact factor: 2.991