Saima Q Memon1, Najma Memon, S W Shah, M Y Khuhawar, M I Bhanger.
Abstract
The ability of sawdust (treated and untreated) waste, a waste material derived from the commercial processing of cedrus deodar wood for furniture production, to remove/preconcentrate Cd(II) ions from aqueous solution was determined. Sorption was found to be rapid (approximately 97% within 8 min). The binding of metal ions was found to be pH dependent, optimal sorption accruing at around pH 4-8. Potentiometric titrations of sawdust revealed two distinct pK(a) values, the first having the value similar to carboxylic groups (3.3-4.8) and second comparable with that of amines (8.53-10.2) with the densities 1.99 x 10(-4) and 7.94 x 10(-5), respectively. Retained Cd(II) ions were eluted with 5 ml of 0.1 mol l(-1) HCl. Detection limit of 0.016 microg ml(-1) was achieved with enrichment factors of 120. Recovery was quantitative using sample volume of 600 ml. The Langmuir and D-R isotherm equations were used to describe partitioning behavior for the system at different temperatures. Kinetic and thermodynamic behavior of sawdust for Cd(II) ions removal was also studied.Entities:
Mesh:
Substances:
Year: 2006 PMID: 16844287 DOI: 10.1016/j.jhazmat.2006.06.013
Source DB: PubMed Journal: J Hazard Mater ISSN: 0304-3894 Impact factor: 10.588