Alfredo Julio Fernandes Neto1, Heitor Panzeri, Flavio Domingues Neves, Ricardo Alves do Prado, Gustavo Mendonça.
Abstract
Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cylinder specimens (15 mm in height; 6 mm in diameter) were obtained for each alloy, in away that 10 specimens of each alloy were tested with each porcelain. Bond strength was measured with an Emic screw-driven mechanical testing machine by applying parallel shear forces to the specimens until fracture. Kruskal-Wallis and Mann-Whitney U tests were used for statistical analysis of the alloy/ceramic combinations (p<0.05). Resistal P/Duceram had significantly higher bond strength (44.38+/-9.12 MPa) (p<0.05) than the other combinations, except for Co-Cr-Ti alloy/Vita VMK 88 (38.41+/-12.64 MPa). The association of the experimental Co-Cr-Ti alloy with Williams porcelain had significantly higher bond strength (28.20+/-3.86 MPa) than the combination of other alloys with the same porcelain (p<0.05). Based of these results and within the limitations of an in vitro study, it may be concluded that the bond strength of the three ceramic systems to the Ni-Cr and Co-Cr-Ti alloys varied significantly, indicating that metal/ceramic compatibility was very important to the bond strength.Entities:
Mesh:
Substances:
Year: 2006 PMID: 16721460 DOI: 10.1590/s0103-64402006000100006
Source DB: PubMed Journal: Braz Dent J ISSN: 0103-6440