| Literature DB >> 15585225 |
M Nakagawa1, Y Matono, S Matsuya, K Udoh, K Ishikawa.
Abstract
In this study, we examined the corrosion behaviors of pure titanium, the alloys Ti-6Al-4V and Ti-6Al-7Nb, and the new experimental alloys Ti-Pt and Ti-Pd using anodic polarization and corrosion potential measurements in an environment containing fluoride. Before and after immersion in the test solutions, we made observations using a scanning electron microscope. The test solutions included an artificial saliva containing 0.2% NaF (corresponding to 905 ppm F) and an artificial saliva with a low concentration of oxygen. Although the surfaces of the Ti-Pt and Ti-Pd alloys were not affected by an acidic environment containing fluoride, the surfaces of the pure titanium, the Ti-6Al-4V alloy, and the Ti-6Al-7Nb alloy were markedly roughened by corrosion. The surfaces of the pure titanium, the Ti-6Al-4V alloy, and the Ti-6Al-7Nb alloy were microscopically damaged by corrosion when they were immersed in the solution containing a low concentration of dissolved oxygen, even with a fluoride concentration included in the commercial dentifrices. In this situation, however, the surfaces of the new Ti-Pt and Ti-Pd alloys were not affected. These alloys are expected to be of use in dental work as new titanium alloys with high corrosion resistances.Entities:
Mesh:
Substances:
Year: 2005 PMID: 15585225 DOI: 10.1016/j.biomaterials.2004.07.022
Source DB: PubMed Journal: Biomaterials ISSN: 0142-9612 Impact factor: 12.479