Metal behavior during vitrification of incinerator ash in a coke bed furnace.

Yi-Ming Kuo1, Ta-Chang Lin, Perng-Jy Tsai.   

Abstract

In this study, municipal waste incinerator ash was vitrified in a coke bed furnace system and the behavior of metals was investigated. Coke and lime were added to provide heat which facilitated vitrification. Ash contributed more than 90% of metal (except for Ca) input-mass. Metal species with low boiling points accounted for the major fraction of their input-mass adsorbed by air pollution control devices (APCDs) fly ash. Among the remaining metals, those species with light specific weights in this furnace tended to be encapsulated in slag, while heavier species were mainly discharged by ingot. Meanwhile, the leachability of hazardous metals in slag was significantly reduced. The distribution index (DI) was defined and used as an index for distribution of heavy metals in the system. A high DI assures safe slag reuse and implies feasibility of recovering hazardous heavy metals such as Cr, Cu, Fe, Pb and Zn. The vitrification in a coke bed furnace proved to be a useful technology for the final disposal of MSW incinerator ash. The heavy metals are separated into the slag, ingot and fly ash, allowing safe reuse of the slag and possible recovery of the metals contained in the ingot and ash fractions.

Entities:  

Mesh:

Substances:

Year:  2004        PMID: 15177748     DOI: 10.1016/j.jhazmat.2004.02.053

Source DB:  PubMed          Journal:  J Hazard Mater        ISSN: 0304-3894            Impact factor:   10.588


  1 in total

1.  Variation and correlation of content and leachability of hazardous metals in MSW molten slag.

Authors:  T Sekito; K Onoue; Y Dote; H Sakanakura; K Nakamura
Journal:  Environ Monit Assess       Date:  2014-12-11       Impact factor: 2.513

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.