| Literature DB >> 15062817 |
W D Wan Rosli1, K N Law, Z Zainuddin, R Asro.
Abstract
Caustic pulping of oil-palm frond-fiber strands was conducted following a central composite design using a two-level factorial plan involving three pulping variables (temperature: 160-180 degrees C, time: 1-2 h, alkali charge: 20-30% NaOH). Responses of pulp properties to the process variables were analyzed using a statistical software (DESIGN-EXPERT). The results indicated that frond-fiber strands could be pulped with ease to about 35-45% yield. Statistically, the reaction time was not a significant factor while the influences of the treatment temperature and caustic charge were in general significantly relative to the properties of the resultant pulps. Copyright 2003 Elsevier Ltd.Entities:
Mesh:
Substances:
Year: 2004 PMID: 15062817 DOI: 10.1016/j.biortech.2003.11.016
Source DB: PubMed Journal: Bioresour Technol ISSN: 0960-8524 Impact factor: 9.642