Literature DB >> 12970665

Plasma arc curing of ceramic brackets: an evaluation of shear bond strength and debonding characteristics.

Arndt Klocke1, Heike M Korbmacher, Lothar G Huck, Joydeep Ghosh, Bärbel Kahl-Nieke.   

Abstract

The aim of this in vitro investigation was to evaluate bond strength and debonding characteristics when a xenon plasma arc curing light is used to bond polycrystalline and monocrystalline ceramic brackets. Brackets were bonded to 240 extracted bovine mandibular incisors with a composite adhesive. Curing intervals of 1, 3, and 6 seconds were chosen for curing with the plasma arc light, and the control group was cured at 10 seconds per bracket with a conventional halogen light. Debonding was performed on a universal testing machine and according to the bracket manufacturers' recommendations. Both the polycrystalline and the monocrystalline brackets consistently debonded at the bracket-adhesive interface, regardless of debonding method, curing interval, or curing light. No enamel fractures were observed after debonding. Bracket fractures were rare and did not affect debonding. Bond strength was significantly higher for the monocrystalline brackets (P <.0001): mean shear bond strength ranged between 9.68 +/- 2.17 MPa (plasma arc curing light, 1 sec curing interval) and 10.73 +/- 3.22 MPa (halogen light, 10 sec curing interval) for the polycrystalline brackets and between 19.85 +/- 2.97 MPa (plasma arc curing light, 1 sec curing interval) and 22.94 +/- 3.20 MPa (plasma arc curing light, 3 sec curing interval) for the monocrystalline brackets. Significant differences were also found for the curing methods used (P =.047). A curing interval of 3 seconds with the plasma arc curing light is recommended for both polycrystalline and monocrystalline ceramic brackets.

Entities:  

Mesh:

Substances:

Year:  2003        PMID: 12970665     DOI: 10.1016/s0889-5406(03)00310-x

Source DB:  PubMed          Journal:  Am J Orthod Dentofacial Orthop        ISSN: 0889-5406            Impact factor:   2.650


  5 in total

1.  Comparison of shear bond strength of plastic and ceramic brackets.

Authors:  V Zielinski; S Reimann; A Jäger; C Bourauel
Journal:  J Orofac Orthop       Date:  2014-08-28       Impact factor: 1.938

2.  Effect of a DPSS laser on the shear bond strength of ceramic brackets with different base designs.

Authors:  Mi-Gyoung Park; Jung-Hoon Ro; Jeong-Kil Park; Ching-Chang Ko; Yong Hoon Kwon
Journal:  Lasers Med Sci       Date:  2012-11-08       Impact factor: 3.161

3.  Effect of Dental Chair Light on Enamel Bonding of Orthodontic Brackets Using Light Cure Based Adhesive System: An In-Vitro Study.

Authors:  Anil Tiwari; Tarulatha Shyagali; Sarvraj Kohli; Rishi Joshi; Abhishek Gupta; Rana Tiwari
Journal:  Acta Inform Med       Date:  2016-11-01

4.  Shear Bond Strength of Rebonded Ceramic Brackets Using Four Different Methods of Adhesive Removal.

Authors:  Amir Hossein Mirhashemi; Mohammad Hashem Hosseini; Nasim Chiniforoush; Armin Soudi; Meisam Moradi
Journal:  J Dent (Tehran)       Date:  2018-01

5.  Comparison of shear bond strength of orthodontic brackets bonded with halogen and plasma arc light curing.

Authors:  Mohammad Hossein Toodehzaeim; Alireza Danesh Kazemi; Hossein Agha Aghili; Kazem Barzegar; Taranom Fallahtafti
Journal:  Dent Res J (Isfahan)       Date:  2012-05
  5 in total