Resin-modified glass ionomer cement and self-cured resin composite luted ceramic inlays. A 5-year clinical evaluation.

Jan W V van Dijken1.   

Abstract

OBJECTIVE: This study evaluated IPS Empress ceramic inlays luted with two chemical-cured luting agents, a resin-modified glass ionomer cement (Fuji Plus (F)) and a resin composite (RC) (Panavia 21 (P)).
METHODS: Seventy-nine ceramic inlays were placed in Class II cavities in 29 patients. At least two inlays were placed in each patient to compare the luting techniques intra-individually. In each patient half of the inlays were luted with F and the other half with P. The inlays were evaluated clinically, according to modified USPHS criteria (van Dijken, 1986), at baseline, after 6 months, and yearly during 5 years.
RESULTS: At 5 years, 71 inlays were evaluated. Two small partial fractures were observed at 3 years (1P, 1F). One inlay showed recurrent root caries at 4 years (P). Four inlays, two in each group showed non-acceptable color match (2P, 2F). Small defects were observed in 4 inlays (2P, 2F). A slight ditching of the cement margins was observed in both luting groups but did not seem to increase during the second half of the evaluation. No significant difference in durability was observed between the two luting agents. SIGNIFICANCE: IPS Empress inlays luted with the chemical-cured RC and the resin-modified glass ionomer cement functioned satisfactory during the 5 years follow-up.

Entities:  

Mesh:

Substances:

Year:  2003        PMID: 12901993     DOI: 10.1016/s0109-5641(03)00011-3

Source DB:  PubMed          Journal:  Dent Mater        ISSN: 0109-5641            Impact factor:   5.304


  6 in total

1.  Seven-year clinical performance of CEREC-2 all-ceramic CAD/CAM restorations placed within deeply destroyed teeth.

Authors:  Matthias J Roggendorf; Bianka Kunzi; Johannes Ebert; Hubert C Roggendorf; Roland Frankenberger; Sven M Reich
Journal:  Clin Oral Investig       Date:  2011-12-07       Impact factor: 3.573

2.  Light curing through glass ceramics with a second- and a third-generation LED curing unit: effect of curing mode on the degree of conversion of dual-curing resin cements.

Authors:  Simon Flury; Adrian Lussi; Reinhard Hickel; Nicoleta Ilie
Journal:  Clin Oral Investig       Date:  2013-02-08       Impact factor: 3.573

3.  Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations.

Authors:  Petra C Guess; Stefan Schultheis; Martin Wolkewitz; Yu Zhang; Joerg R Strub
Journal:  J Prosthet Dent       Date:  2013-10       Impact factor: 3.426

4.  Marginal integrity of CAD/CAM fixed partial dentures.

Authors:  Martin Rosentritt; Michael Behr; Carola Kolbeck; Gerhard Handel
Journal:  Eur J Dent       Date:  2007-01

5.  Healing of Oral Lichenoid Lesions following Replacement of Dental Amalgam Restorations with Feldspathic Ceramic Inlay-Onlay Restorations: Clinical Results of a Follow-Up Period Varied from Three Months up to Five Years.

Authors:  Burcin Karatasli; Gokcen Karatasli; Ozgur Mete; Mehmet Ali Erdem; Abdulkadir Burak Cankaya
Journal:  Biomed Res Int       Date:  2018-12-03       Impact factor: 3.411

Review 6.  Cementation of Glass-Ceramic Posterior Restorations: A Systematic Review.

Authors:  Carline R G van den Breemer; Marco M M Gresnigt; Marco S Cune
Journal:  Biomed Res Int       Date:  2015-10-18       Impact factor: 3.411

  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.