The effect of curing with plasma light on the shrinkage of dental restorative materials.

S Deb1, R Mallett, B Millar.   

Abstract

Commercially available light activated dental composites were used in this study to compare the shrinkage following curing with plasma light (Apollo95E, DMDS) and a convention halogen dental curing light (Prismetics Lite II, Dentsply). Polymerization shrinkage was determined by measuring the strain in one dimension by means of a contacting transducer. The percentage linear shrinkage were: Spectrum H = 1.84 + 0.31, P = 1.49 + 0.35*; Ana aesthetic H = 2.04 + 0.38, P = 1.85 + 0.27; Esthet.x H = 1.66 + 0.28, P = 1.69 + 0.25; Dyract AP H = 2.39 + 0.33, P = 2.18 + 0.35*; Apollo Restore H = 1.88 + 0.36, P = 1.42 + 0.33*; Surefil H = 0.88 + 0.28, P = 0.99 + 0.30 where * = significantly different, t-test at P < 0.05. The results suggested that there was less shrinkage when curing some, but not all, materials using the plasma light, although this could be attributed to a reduced level of polymerization.

Mesh:

Substances:

Year:  2003        PMID: 12791159     DOI: 10.1046/j.1365-2842.2003.01128.x

Source DB:  PubMed          Journal:  J Oral Rehabil        ISSN: 0305-182X            Impact factor:   3.837


  1 in total

1.  Influence of light-curing procedures and photo-initiator/co-initiator composition on the degree of conversion of light-curing resins.

Authors:  N Emami; K-J M Söderholm
Journal:  J Mater Sci Mater Med       Date:  2005-01       Impact factor: 3.896

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.