Hydrothermal and pulp processing of Eucalyptus.

G Garrote1, M E Eugenio, M J Díaz, J Ariza, F López.   

Abstract

Hydrothermal processing of Eucalyptus wood was performed at operation temperature of 181 degrees C, processing time or 37.5 min and solid water ratio of 1/6 to ensure a maximum loss of xylan recuperation with minimum cellulose fibre degradation. Under those conditions, the loss of xylan was 22% less than that achieved with the conditions 196 degrees C, 50.6 min and 1/8 (solid/water). IN In addition, an experimental design was used to study the influence of process variables: temperature (145-175 degrees C), pulping time (40-120 min) and ethanol concentration (40-70% weight concentration), on the properties of pulps (yield, kappa number, viscosity, cellulose, xylan, lignin acetyl groups contents and brightness) and paper sheets (stretch index, burst index and tear index) obtained from the solid fraction after hydrothermal treatment of Eucalyptus globulus. Pulps with acceptably high physical and chemical properties can be obtained operating at 175 degrees C for 90 min with 55% ethanol concentration.

Entities:  

Mesh:

Substances:

Year:  2003        PMID: 12573565     DOI: 10.1016/s0960-8524(02)00256-0

Source DB:  PubMed          Journal:  Bioresour Technol        ISSN: 0960-8524            Impact factor:   9.642


  1 in total

1.  Structural and chemical characterization of hardwood from tree species with applications as bioenergy feedstocks.

Authors:  Özgül Persil Cetinkol; Andreia M Smith-Moritz; Gang Cheng; Jeemeng Lao; Anthe George; Kunlun Hong; Robert Henry; Blake A Simmons; Joshua L Heazlewood; Bradley M Holmes
Journal:  PLoS One       Date:  2012-12-28       Impact factor: 3.240

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.