Literature DB >> 11856389

Adhesive bonding of composite material to cast titanium with varying surface preparations.

H Yanagida1, H Matsumura, Y Taira, M Atsuta, S Shimoe.   

Abstract

The purpose of the present study was to evaluate the surface preparation effects of eight metal conditioners and an adhesive system on bonding between a prosthodontic composite material and cast titanium. Eight primers designed for conditioning base metal alloys (Acryl Bond, All-Bond 2 Primer B, Alloy Primer, Cesead II Opaque Primer, Eye Sight Opaque Primer, Metafast Bonding Liner, Metal Primer II, and MR Bond) as well as a surface modification technique (Siloc) were assessed. Disk specimens cast from titanium (T-Alloy H) were either primed with one of the eight primers or treated with the Siloc system, and then bonded with a light-activated composite material (Artglass). Bond durability was evaluated by thermocycling (4 and 60 degrees C, 1 min each, 20, 000 cycles). After thermocycling, two groups either primed with the Cesead II Opaque Primer material or treated with the Siloc system exhibited significantly greater bond strength (20.0 and 19.0 MPa) than the other groups (0.2-12.6 MPa, P < 0.05). These two systems are considered to be useful for improving bonding between the titanium and the composite material tested.

Entities:  

Mesh:

Substances:

Year:  2002        PMID: 11856389     DOI: 10.1046/j.1365-2842.2002.00811.x

Source DB:  PubMed          Journal:  J Oral Rehabil        ISSN: 0305-182X            Impact factor:   3.837


  6 in total

1.  Resistance to cyclic loading of teeth restored with posts.

Authors:  A Sahafi; A Peutzfeldt; G Ravnholt; E Asmussen; K Gotfredsen
Journal:  Clin Oral Investig       Date:  2005-03-04       Impact factor: 3.573

2.  Evaluation of two dual-functional primers and a tribochemical surface modification system applied to the bonding of an indirect composite resin to metals.

Authors:  Hiroaki Yanagida; Naomi Tanoue; Takako Ide; Hideo Matsumura
Journal:  Odontology       Date:  2009-07-29       Impact factor: 2.634

3.  Effect of Fiber Laser Irradiation on the Shear Bond Strength between Acrylic Resin and Titanium.

Authors:  Fatih Mehmet Korkmaz; Selin Aycan
Journal:  Scanning       Date:  2019-09-03       Impact factor: 1.932

4.  Factors affecting the bond strength of denture base and reline acrylic resins to base metal materials.

Authors:  Naomi Tanoue; Yasuhiro Matsuda; Hiroaki Yanagida; Hideo Matsumura; Takashi Sawase
Journal:  J Appl Oral Sci       Date:  2013 Jul-Aug       Impact factor: 2.698

5.  Adhesive bonding of resin composite to various titanium surfaces using different metal conditioners and a surface modification system.

Authors:  Hercules Jorge Almilhatti; Karin Hermana Neppelenbroek; Carlos Eduardo Vergani; Ana Lúcia Machado; Ana Cláudia Pavarina; Eunice Teresinha Giampaolo
Journal:  J Appl Oral Sci       Date:  2013 Nov-Dec       Impact factor: 2.698

6.  The effect of continuous application of MDP-containing primer and luting resin cement on bond strength to tribochemical silica-coated Y-TZP.

Authors:  Myung-Jin Lim; Mi-Kyung Yu; Kwang-Won Lee
Journal:  Restor Dent Endod       Date:  2018-04-03
  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.