Fracture resistance of teeth restored with the bonded amalgam technique.

G M Dias de Souza1, G D Pereira, C T Dias, L A Paulillo.   

Abstract

This study evaluated the fracture resistance of maxillary premolars with MOD Class II cavity preparations restored with silver amalgam (G1), Scotchbond Multi Purpose Plus and silver amalgam (G2) and Panavia F and silver amalgam (G3). After the restorations were made, the specimens were stored at 37 degrees C for 24 hours at 100% humidity and submitted to the compression test. Statistical analysis of the data (ANOVA and Tukey Test) revealed no significant differences among the three groups that were studied.

Entities:  

Mesh:

Substances:

Year:  2001        PMID: 11551017

Source DB:  PubMed          Journal:  Oper Dent        ISSN: 0361-7734            Impact factor:   2.440


  2 in total

1.  Cusp fracture resistance of maxillary premolars restored with the bonded amalgam technique using various luting agents.

Authors:  Shivaughn M Marchan; Larry Coldero; Daniel White; William A J Smith; Reisha N Rafeek
Journal:  Int J Dent       Date:  2008-12-25

2.  Effect of composite/amalgam thickness on fracture resistance of maxillary premolar teeth, restored with combined amalgam-composite restorations.

Authors:  Maryam Firouzmandi; Maryam Doozandeh; Zahra Jowkar; Sanaz Abbasi
Journal:  J Clin Exp Dent       Date:  2016-07-01
  2 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.